I believe they are no longer being imported , and I don't have a tumbler or moly kit. Does anyone have any they don't want? I'll pay $46 per 100 plus postage for unopened boxes (that is the price SARA had them for).
-
- Posts: 166
- Joined: Sun Jun 19, 2005 10:40 am
- Location: South Australia
G'day Alan
I checked Grafs and Sinclair and they don't appear to stock the moly ones. 1000 naked Scenars is only US$198.99 from Grafs and they only charge US$50 for processing the export license http://www.grafs.com/orderingInfo.cfm so you could try asking them about the moly ones. I think the guy who deals with exports is Matt export@grafs.com
Regards
Ben
PS The uncoated ones work pretty well for me if Grafs can't get you moly ones.
I checked Grafs and Sinclair and they don't appear to stock the moly ones. 1000 naked Scenars is only US$198.99 from Grafs and they only charge US$50 for processing the export license http://www.grafs.com/orderingInfo.cfm so you could try asking them about the moly ones. I think the guy who deals with exports is Matt export@grafs.com
Regards
Ben
PS The uncoated ones work pretty well for me if Grafs can't get you moly ones.
Re: 6.5 139gr Moly Scenars Wanted
AlanF wrote:I believe they are no longer being imported , and I don't have a tumbler or moly kit. Does anyone have any they don't want? I'll pay $46 per 100 plus postage for unopened boxes (that is the price SARA had them for).
Alan, I have plenty of 139's uncoated if you are stuck.
Nick Simms
simms@connexus.net.au
-
- Posts: 411
- Joined: Wed Jun 22, 2005 1:29 pm
- Location: Goulburn NSW Australia
139 Scenars - moly
Try Mick Helm from Southern Highlands club. He may have 2x100. He has switched to a 6 BR. He lives near PICTON NSW and is listed in the phone book. Also ask him for contact at "Stagearms" as they may have some in stock.
-
- Site Admin
- Posts: 39
- Joined: Mon Apr 25, 2005 9:44 pm
-
- Posts: 102
- Joined: Mon Jun 20, 2005 12:25 pm
- Location: Perth
Alan
Perhaps you should try coating your own. I have a Hoover tumbler - the one the washing gets dried in! I put 2-300 naked ones in a small Milo tin (or similar), add 1/4 teaspoon high grade moly powder, shut it tight and seal it with tape (marriage limiting event if it comes undone), and then pack it well in the dryer with blankets and pillows so it won't move too much. I give mine 2 goes at 30 minutes each - the amount of time on the cool down cycle - and all is done. Hard to tell apart from the bought ones.
I pour them onto an old t-shirt or tea towel, roll them around to remove loose powder, then pack them back into their packets.
The idea came from my wife when she saw me looking at kids prams, old washing machine motors etc with a view to creating a contraption for the tumbling.
I'll buy mine coated if I can. I couldn't get coated last I bought either.
Good luck.
Mark Hamersley
Perhaps you should try coating your own. I have a Hoover tumbler - the one the washing gets dried in! I put 2-300 naked ones in a small Milo tin (or similar), add 1/4 teaspoon high grade moly powder, shut it tight and seal it with tape (marriage limiting event if it comes undone), and then pack it well in the dryer with blankets and pillows so it won't move too much. I give mine 2 goes at 30 minutes each - the amount of time on the cool down cycle - and all is done. Hard to tell apart from the bought ones.
I pour them onto an old t-shirt or tea towel, roll them around to remove loose powder, then pack them back into their packets.
The idea came from my wife when she saw me looking at kids prams, old washing machine motors etc with a view to creating a contraption for the tumbling.
I'll buy mine coated if I can. I couldn't get coated last I bought either.
Good luck.
Mark Hamersley
-
- Posts: 7502
- Joined: Wed Jun 15, 2005 8:22 pm
- Location: Maffra, Vic
-
- Posts: 277
- Joined: Fri Jun 17, 2005 8:05 pm
Hi all
I used to coat my own and i used to put approx 25-50 bullets along with some3/16 ball bearings and i/s teaspoon of moly powder from industrial supplies all into a screw top glass baby food jar and place three or four of them into my vibrating case cleaner along with the cleaning media. Leave them in for approx 1 hr. The time all depends on how many bullets are in the jar. You will have to judge this for yourself. Once done sift bullets from bearings and left over moly powder, tip bullets onto cloth and wipe off excess. Tip bearings and powder into jar ready for next time.
Paul
I used to coat my own and i used to put approx 25-50 bullets along with some3/16 ball bearings and i/s teaspoon of moly powder from industrial supplies all into a screw top glass baby food jar and place three or four of them into my vibrating case cleaner along with the cleaning media. Leave them in for approx 1 hr. The time all depends on how many bullets are in the jar. You will have to judge this for yourself. Once done sift bullets from bearings and left over moly powder, tip bullets onto cloth and wipe off excess. Tip bearings and powder into jar ready for next time.
Paul
-
- Posts: 102
- Joined: Mon Jun 20, 2005 12:25 pm
- Location: Perth
Alan
A fellow club member got some moly powder years ago and divvied it up into film canisters. I'm pretty sure he got it from an industrial supplier.
I don't use shot or ball bearings, just naked bullets plus about a level teaspoon for each 2-300. It works for me. My tin ends up about 2/3 full of bullets, you need space for them to tumble against each other in the tin.
Paul's approach is sounds better, I think the ball bearings would improve the efficiency of the process. As Paul says, recover what you can for future use and play with the timing.
You also need to make sure the dryer is packed well. If the tin is well centred it should be OK, otherwise it can get a bad case of the shakes.
Good luck!
Mark Hamersley
A fellow club member got some moly powder years ago and divvied it up into film canisters. I'm pretty sure he got it from an industrial supplier.
I don't use shot or ball bearings, just naked bullets plus about a level teaspoon for each 2-300. It works for me. My tin ends up about 2/3 full of bullets, you need space for them to tumble against each other in the tin.
Paul's approach is sounds better, I think the ball bearings would improve the efficiency of the process. As Paul says, recover what you can for future use and play with the timing.
You also need to make sure the dryer is packed well. If the tin is well centred it should be OK, otherwise it can get a bad case of the shakes.
Good luck!
Mark Hamersley
Return to “Equipment & Technical”
Who is online
Users browsing this forum: No registered users and 74 guests